Computational Modeling of Nanoindentation
Kovář, Jaroslav ; Čech,, Jaroslav (referee) ; Dlouhý, Ivo (referee) ; Fuis, Vladimír (advisor)
Doctoral thesis is aimed on the computation modelling of a nanoindentation test. The informa-tional research of nanoindentation test and analytical models, which were used for derivation of the formulas for evaluation of measured data, is done in the introduction. Analytical models were derived with few simplifying assumptions, whose influence was analyzed in the computa-tional part of the thesis. This part is aimed on the computational modelling of nanoindentation test with the use of finite element method, especially the nanoindentation test of fused silica, steel and thin layers deposited on substrate. These models were used for refinement of calculations by the influence of radial displacements under the tip of indenter and correction coefficient for the indenter shape. In the next part, the influence of the indenter bluntness and tilt on its shape function was analyzed. The last part of the thesis dealing with thin layers was aimed on the verification of one tenth rule of thumb for determination of reduced modulus and hardness with the blunted and ideal Berkovich indenter.
|
|
Surface and mechanical properties of a-CSi:H and a-CSiO:H films
Plichta, Tomáš ; Shukurov, Andrey (referee) ; Klapetek, Petr (referee) ; Čech, Vladimír (advisor)
The dissertation thesis deals with the preparation and characterisation of a-CSi:H and a CSiO:H thin films prepared using the process of plasma enhanced chemical vapour deposition (PECVD). Tetravinylsilane (TVS) and its mixtures with argon and oxygen were used to deposit films on both planar substrates and fibre bundles. Main characterisation techniques were employed to study the topography of films, namely atomic force microscopy (AFM). Their mechanical properties were studied through nanoindentation; the nanoscratch test was used to assess the film adhesion to the substrate. Other analysed properties were internal stress and friction coefficient. The particular attention was paid to the work of adhesion and its determination. This knowledge was further applied to the preparation of surface treatments of glass fibres and, subsequently, polymer composites. Those were tested using the push-out test and the short beam shear test. Based on the results, the effects of deposition conditions and the relationships between the studied properties and quantities were determined.
|
|
THE APPLICATION OF NANOMATERIALS FOR LEAD FREE SOLDERS DEVELOPMENT
Pešina, Zbyněk ; Pinkas, Jiří (referee) ; Spousta, Jiří (referee) ; Sopoušek, Jiří (advisor)
The present dissertation is motivated by the search for alternatives of lead-free soldering by nanoparticles of metals and their alloys. The research focuses on the possibility of replacing lead-free solders by nanoparticles. This issue is currently being addressed by the use of lead-free solders but their properties are not entirely equivalent to properties of lead-tin based alloys. The theoretical part of the dissertation first summarizes up-to date knowledge on the development of lead-free alloys currently used for soldering in the electronics. The work compares these lead-free solder candidates with previously used Pb-Sn alloys. The second section of the theoretical part is devoted to nanotechnology that offers possible solutions of problems associated with the use of lead-free solders. The text contains a description of the properties of nanocrystalline materials in comparison with those of compact alloys having the same chemical composition. The possibility of preparation of nanoparticles and potential problems associated with small particle sizes are also presented. Introduction of the experimental part focuses on the preparation of nanoparticles of pure metals and alloys by chemical and physical ways as well as on an instrumentation for characterisation and analysis. Attention is focused on the silver in nanoparticle form that exhibits the low temperature sintering effect, which is thermally activated by decomposition of oxide envelope covering the Ag nanoparticles. This factor is critical for low-temperature sintering and thus also for possible future applications. The thermal effects of the low sintering process were studied by methods of thermal analysis. The preparation of the Cu / Ag nano / Cu joints was carried out in-situ in inert atmosphere and under the action of atmospheric oxygen. In both cases varying conditions of thermal treatment were used. The cross sections of the prepared joints were then used for the metallographic analysis of the local mechanical properties of the resulting silver layer, for the chemical composition evaluation of the resulting layers of the joint, and for the microstructure study. Strength characteristics are represented by testing shear strength of individual joints.
|
|
Surface analysis of xGnP/PEI nanocomposite
Červenka, Jiří ; Klapetek, Petr (referee) ; Čech, Vladimír (advisor)
Tato Diplomová práce se zabývá povrchovou analýzou nanokompozitní folie polyetherimidu (PEI) vyztuženého exfoliovanými grafitickými nanodestičkami (xGnP). Analyzovány byly take vzorky nevyztužené PEI folie a samostatné nanodestičky. Vzorky nanokompozitu a PEI folie byly plazmaticky leptány s využitím argonového plazmatu po dobu 1, 3 a 10 hod. Skenovací elektronová mikroskopie (SEM) byla použita pro charakterizaci samostatných nanodestiček rozptýlených na křemíkovém substrátu, původních či leptaných vzorků PEI folie a nanokompozitu. Nanodestičky byly identifikovány při povrchu leptané nanokompozitní folie. Mikroskopie atomárních sil (AFM) byla použita pro zobrazení povrchové topografie separovaných nanodestiček a odkrytých destiček při povrchu leptaného kompozitu. Povrchová drsnost (střední kvadratická hodnota, vzdálenost nejnižšího a nejvyššího bodu) leptaného nanokompozitu narůstala s prodlužující se dobou leptání. Akustická mikroskopie atomárních sil (AFAM) byla použita pro charakterizaci elastické anizotropie leptaných kompozitních vzorků. Nanoindentační měření umožnila charakterizaci lokálních mechanických vlastností PEI a nanokompozitních folií.
|
|
Characterisation of Nanostructure Deposited by PVD and CVD Technology
Fořt, Tomáš ; Boušek, Jaroslav (referee) ; RNDr.Vilma Buršíková, Ph.D. (referee) ; Sobota, Jaroslav (advisor)
The thesis deals with mechanical properties of thin hard wear-resistant coatings. The work presents a method of dynamic testing of thin hard coatings on a newly constructed prototype of impact wear tester. It provides a comparison with standard methods of layer testing and presents new experimental results of dynamic impact wear test of the coatings. Finally, the thesis covers preparation techniques of thin film systems deposited on various substrates and their characterization using optical and electron microscopy.
|
|
Wood microstructure analysis onto the strength parameters
Martinek, Radomír ; Kuklík,, Pavel (referee) ; Vaněrek, Jan (advisor)
This work focuses on a closer examination of the microstructure of wood and the relationship between microscopic and mechanical properties of wood. The main point of the practical part of this study is a measurement of microfibril angle (MFA) in the S2 layer of a wood cell wall. This layer occupies more than 80 % of the total thickness of the cell wall and thus has the greatest influence on the mechanical properties of the wood cells. MFA values as well as values of bulk density show a strong dependence on the modulus of elasticity in the longitudinal direction, as well as on the values of shrinkage. The theoretical part involves methods for measuring MFA, variations of MFA, wood properties evolving from the MFA and also mechanical properties of wood cell walls measured by nanoindentation.
|
|
Fracture of selected building composites in the vicinity of aggregate-matrix-interface
Vyhlídal, Michal ; Malíková, Lucie (referee) ; Keršner, Zbyněk (advisor)
The interface between aggregate grains and matrix in cementitious composites is their weakest element. The topic is particularly significant in the case of high performance and high strength concrete technology for which the eliminination or reduction of these weak links are necessary. The aim of this thesis is to determine the influence of the interface on the fracture behaviour of the cementitious composites. The fracture experiments were performed for this purpose and were complemented by the nanoindentation’s results and scanning electron microscopy results. Numerical model was created in ANSYS software on the basis of these data and the fracture toughness values of the interface were evaluated by means of the generalized fracture mechanics principles. Conclusion of the thesis is proof that the interface properties have a significant influence on the fracture behaviour of cementitious composites.
|
|
Development of Nanofabrication Methodology for Study of Mechanical Properties of Thin Films using Focused Ion Beams
Kuběna, Ivo ; Švejcar, Jiří (referee) ; Kruml, Tomáš (advisor)
The main goal of this work is to find a methodology of the fabrication of microcompressive specimens (pillars) from thin metallic film prepared by means of PVD. The studied film was prepared by the ON Semiconductor company, Roznov pod Radhostem. Its chemical composition was Al-1.5 wt.% Cu; such films are used for electric connections on integrated circuits. At first, a thin intermediate layer of W-10 wt.% Ti was deposited on the Si single crystalline substrate with the purpose of improving adhesion properties of the studied film. The geometry of the microcompressive specimen should be as close to the cylindrical shape as possible. The height of the cylinder is given by the film thickness, its diameter is approximately 1 m. Such specimens were prepared in Quanta 3D FEG Dual BeamTM facility using focused ion beams technology. Experiments were done at FEI Company in Brno. In total, 39 microcompressive specimens were prepared at various ion milling conditions. The required geometry was finally attained by the optimization of processing parameters, in particular the parallelism of lateral faces was improved, the bottom of the removed zone in the vicinity of the pillar was almost flat and the transition pillar – flat bottom was regular. The prepared pillars are suitable for the microcompression tests; the first of them have been already performed within the cooperation with the Institut of Physics, Academy of Sciences of the Czech Republic, Praha.
|
|
Surface topography and mechanical properties of thin films on tetravinylsilane basis
Plichta, Tomáš ; Klapetek, Petr (referee) ; Čech, Vladimír (advisor)
Proposed diploma thesis is focused on preparation and characterization of the plasma polymer thin films based on tetravinylsilane monomer (TVS). Plasma enhanced chemical vapour deposition (PECVD) method involving pulse and continual plasma discharge modes were used for thin film deposition on silicon wafer pieces. Reactive plasma composition was containing pure TVS or mixtures of TVS and argon or oxygen gas. Atomic force microscopy was used for surface topography and roughness characterization. Cyclic nanoindentation was involved to measurements to determine the Young’s modulus and hardness of prepared films and scratch test was performed to evaluate the degree of adhesion. Special attention was drawn to the characterization of films with a Young’s modulus below 10 GPa. Tip geometry of indenter influence on scratch test was also commented. Surface and mechanical properties of thin films in relation to the deposition conditions were correlated to the obtained results and final analysis of deposition conditions influence is proposed.
|
|
Advanced techniques in nanoindentation testing
Břečka, Jan ; Tkachenko, Serhii (referee) ; Čížek, Jan (advisor)
The aim of this thesis is to determine the suitability of using advanced indentation methods for various materials. These advanced measurement methods are described in detail and subsequently compared in terms of time complexity and accuracy of the elastic modulus and the hardness measurement. The tested materials were copper and silica. The comparison of the methods is carried out at different views and gives a general overview of advantages of these methods.
|